logo

PIN MALE CONTACTOR WHITE TOYOTA Air Jet Loom Part HL1203-001 68800-09006 Terminal

Place of Origin: Shanghai, China
Brand Name: Y&H China
Certification: Good Quality
Model Number: Loom wiring harness application - confirmed by photo
Product Details
Place of Origin:
Shanghai, China
Brand Name:
Y&H China
Certification:
Good Quality
Model Number:
Loom wiring harness application - confirmed by photo
Minimum Order Quantity:
100 Pieces
Price:
Request a Quote
Standard Packaging:
Bagged by quantity in neutral export carton
Delivery Time:
5 working days for stock items
Payment Terms:
L/C, D/A, D/P, T/T
Specifications
Item Code:
HL1203-001
Original Part Number:
68800-09006
Reference:
HL1203-001
Product Type:
Male Crimp Terminal
Series:
White Connector Series
Supplied As:
Loose Terminals For Crimping
Related Parts:
HL1202 Female Housing, HL1203 Male Housing
Testing:
Spring And Lance Dimensions Checked; Sample Crimps Pulled To Destruction
Use:
Toyota Air Jet Loom Wiring Harnesses
HS Code:
8536900090
Service:
24-Hour Online Service
Video Outgoing-Inspection:
Provided
Warranty:
Case-by-case
Key Markets:
Southeast Asia, Central Asia, South America, North America, Europe
Shipping:
Express (DHL/FedEx/UPS) / Sea Freight / Air Freight
Brand Name:
Y&H China
Product Description

Product Overview

Male crimp terminal for the white connector series. Original part number 68800-09006, item code HL1203-001, reference HL1203-001. Supplied loose for crimping to the harness.

Terminals are the cheapest component in the cabinet and the one that decides whether a connection lasts ten years or ten weeks. The housing gets the attention; the crimp does the work.

Applications & Compatibility

  • Type: male crimp terminal, white connector series
  • Original part number: 68800-09006
  • Our item code: HL1203-001
  • Reference: HL1203-001
  • Related parts: HL1202 female housing, HL1203 male housing

Confirm the gauge range and the housing series before ordering. Terminals that look similar differ in wire range and in the spring that holds them in the housing.

A Crimp Is Not a Squeeze

  • Strands outside the barrel - the joint carries less current than the wire, and it heats at the terminal rather than at the load.
  • Insulation inside the barrel - the crimp holds plastic, not copper, and it pulls apart under vibration.
  • Over-crimping - nicked strands break one by one, which is why the fault appears months later and never at the bench.
  • A correct crimp shows a bell mouth at both ends - and a few strands visible past the barrel, not cut flush.
  • Pull test every contact you cannot see afterwards - a firm tug costs a second; a backed-out terminal costs a shift.

Most intermittents on a loom harness are not broken wires. They are crimps that were made with the wrong die, or with the insulation stripped to the wrong length, and then passed around by hand.

Keep a Box of Terminals in Stores

  • A terminal costs less than the labour to find one - and far less than a harness.
  • Repair a connector, not a harness - a single failed contact should end with a new contact, not a splice in a moving cable.
  • Do not mix series in one housing - terminals from a different family may insert and then not lock, or lock and not conduct.
  • Use the extraction tool - pulling a terminal out with pliers damages the housing cavity and the next contact will not lock either.
  • Keep the reel or the bag labelled - loose terminals in an unlabelled drawer end up in the wrong housing on a night shift.

A mill with a stocked terminal box solves most harness faults in twenty minutes. A mill without one splices, and then finds the splice two years later in a different place.

Quality Standard

  • Terminal supplied to the original part number with the correct wire range and plating.
  • Spring and locking lance dimensions checked against the reference on each batch.
  • Sample crimps pulled to destruction to confirm die and terminal compatibility.
  • Plating and base metal inspected for discolouration or contamination before packing.
  • Bagged by quantity and marked with the reference; batch recorded.
  • Warranty against manufacturing defects, assessed case by case; damage from incorrect crimping, wrong die, soldering, corrosion from moisture or damage during extraction is not covered.

Air jet loom spare part quality inspection and stability test

Specifications

ProductMale crimp terminal
Original Part Number68800-09006
Item CodeHL1203-001
ReferenceHL1203-001
SeriesWhite connector series
Supplied AsLoose terminals for crimping
TestingSpring and lance dimensions checked; sample crimps pulled to destruction
HS Code8536900090
Place of OriginShanghai, China

Order & Shipping Information

  • Minimum order quantity: 100 pieces.
  • Sample order is acceptable for quality evaluation.
  • Stock items ship within 5 working days after payment confirmation.
  • Bagged by quantity in a neutral export carton.
  • Shipping option: DHL / FedEx / UPS express, air freight, sea freight.
  • Complete export documents including commercial invoice and packing list will be supplied.
  • We ship worldwide to textile markets across Southeast Asia, Central Asia, South America, North America and Europe.

Air jet loom spare part export packing and shipping

Frequently Asked Questions

Q1: Can these be used in any white housing?
Only in the matching series. A terminal from another family may insert without locking, which fails under vibration rather than at the bench.

Q2: What does a good crimp look like?
A bell mouth at both ends of the barrel and a few strands visible past it. Insulation inside the barrel or strands outside are both rejects.

Q3: The terminal pulled out of the housing. Was it faulty?
Usually the locking lance was not engaged, or the cavity was damaged by a previous extraction with pliers.

Q4: Can a terminal be soldered instead of crimped?
It can be made to work and will crack where the strands end. For a harness on a moving machine, crimp and pull test.

Q5: How is the warranty handled?
Manufacturing defects are covered case by case. Damage from incorrect crimping, wrong die, soldering, corrosion or extraction damage is excluded.